The preferred applications for this series are via he encapsulation of:
More
- MC 62 BK Resin and W 363 Hardener is a two component filled epoxy system, fluid. Self-extinguishing. The system is free from halogens and solvens.
- Good electrical and mechanical properties.
- Low shrinkage
- Good heat dissipation
- Suitable for immersion in sea water.
- RoHS compliant (European directive 2002/95/EC).
- fulfills the requirements of UNI-CEI 11170-3 “Protection towards fire of rail-tramvehicles”.
The preferred applications for this series are via he encapsulation of:
- Transformers
- Igniters
- Submersible pumps
- Elnoise filters
- In pre-filled products it is good practice to check and carefully rehomogenize the material if some settling is present. Add he appropriate quantity of hardener o he resin, mix carefully.
- Avoid air trapping. For some applications it can be useful o pre-heat the components and/ or carry out a de-aeration step under vacuum of the mixture before casting.
- For a room temperature curing system postcuring allows fast stabilization of the material and obtainment of he best electrical and mechanical properties. During he curing process I is advisable o avoid thermal variations higher than 10℃/ hour
- Refer to Elantas Malaysia Material Safety Data Sheet(SDS) for MC 62 BK Resin and W 363 Hardener.
- Filled epoxy resins and relative hardeners can be stored for one year and two years respectively, in the original sealed containers, stored in a cool, dry place. After that period or if the material has been stored in anomalous conditions, pre-filled resins can be settled down and their use is possible, only if they are accurately re-homogenized with the help, if necessary, of a mechanical mixer. The hardeners are moisture sensitive therefore it is good practice to close the vessel immediately after each use. Long storage may cause filler settling mix the components before use.
More